File:Weld image of inconel superalloy after destructive tensile test.png

From testwiki
Jump to navigation Jump to search
Original file (815 × 155 pixels, file size: 172 KB, MIME type: image/png)

This file is from Wikimedia Commons and may be used by other projects. The description on its file description page there is shown below.

Summary

Description
English: Weld image of inconel 600 and inconel 718 superalloy after destructive tensile test.
Date
Source

"Rotary Friction Welding of Inconel 718 to Inconel 600"

Department of Industrial Engineering, College of Engineering, King Saud University, Riyadh 11451, Saudi Arabia

Academic Editor: Yutaka S. Sato Metals 2021, 11(2), 244

https://doi.org/10.3390/met11020244
Author Ateekh Ur Rehman, Yusuf Usmani, Ali M. Al-Samhan, Saqib Anwar

Licensing

w:en:Creative Commons
attribution share alike
This file is licensed under the Creative Commons Attribution-Share Alike 4.0 International license.
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
  • share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.

Captions

Weld image of inconel 600 and inconel 718 superalloy after destructive tensile test.

Items portrayed in this file

depicts

14 May 2021

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current21:56, 14 May 2021Thumbnail for version as of 21:56, 14 May 2021815 × 155 (172 KB)wikimediacommons>Xyz00030280Uploaded a work by Ateekh Ur Rehman, Yusuf Usmani, Ali M. Al-Samhan, Saqib Anwar from "Rotary Friction Welding of Inconel 718 to Inconel 600" Department of Industrial Engineering, College of Engineering, King Saud University, Riyadh 11451, Saudi Arabia Academic Editor: Yutaka S. Sato Metals 2021, 11(2), 244 https://doi.org/10.3390/met11020244 with UploadWizard

The following page uses this file: